CNC Turning 5086 Aluminum

VT machining offers CNC Turning for 5086 Aluminum (UNS A95086 / EN AW-5086), typically supplied H32 / H116. Between 5052 and 5083 in strength; excellent seawater resistance.

CNC Turning Notes for 5086 Aluminum

5086 Aluminum turns with good chip control at standard cutting data.

For estimating, a 100 × 100 × 10 mm block of 5086 Aluminum weighs about 0.27 kg.

Starting Parameters for CNC Turning 5086 Aluminum

Cutting speed (carbide)400-1000 m/min
Feed0.1-0.4 mm/rev
Spindle speed, Ø25 mm bar5090-12730 rpm
Insert / tool classISO N — sharp, polished, uncoated or DLC
CoolantEmulsion or MQL; polished uncoated or DLC tools

Starting values for 5086 Aluminum, H32 / H116; optimised on the first article.

5086 Aluminum Data Relevant to CNC Turning

Equivalent designationsUNS A95086 / EN AW-5086
Key compositionMg 3.5-4.5%
Typical supply conditionH32 / H116
Hardness (typical)~70 HB

Typical values; we work to your drawing and mill certificate.

How 5086 Aluminum Differs

Between 5052 and 5083 in strength; excellent seawater resistance.

Typical applications: Boat hulls, marine structures.

5086 Aluminum vs Similar Grades

5086 Aluminum5083 Aluminum5754 Aluminum5052 Aluminum
Key compositionMg 3.5-4.5%Mg 4-4.9%, Mn 0.4-1%Mg 2.6-3.6%Mg 2.2-2.8%, Cr
Hardness~70 HB~75 HB~55 HB~60 HB
Tensile (MPa)~290~290-330~220~230
Typical useBoat hulls, marine structuresShipbuilding, cryogenic tanks, tooling plateAutomotive panels, floor plate, flangesSheet-metal enclosures, marine parts, fuel tanks

More on CNC Turning Aluminum

Finishing options, quality documentation and general cnc turning guidance for all aluminum grades are on our CNC Turning Aluminum page.

Quoting CNC Turning 5086 Aluminum

Send a STEP/IGES model or PDF drawing, confirm 5086 Aluminum and its condition (we usually see it supplied H32 / H116), the quantity, critical tolerances and any finish or certificate requirements.

5086 Aluminum in Other Processes

Related

Send the drawing, the 5086 Aluminum condition and the quantity — pricing and lead time come back the same or next business day.

Request a Quote

Frequently Asked Questions

What surface finish is achievable on 5086 Aluminum with CNC Turning?

Surface finish on 5086 Aluminum is controlled to your specification; we confirm the achievable Ra against your callout.

What tolerances can you hold for CNC Turning 5086 Aluminum?

Achievable tolerances for 5086 Aluminum turning depend on the alloy, geometry and feature size. Turning holds diameter tolerances to around ±0.005 mm with concentricity within 0.01 mm. Exact figures are confirmed against your drawing callouts.

What is the typical lead time and minimum order for CNC Turning 5086 Aluminum?

CNC Turning prototypes for 5086 Aluminum can be produced quickly and scaled to series production. Send your drawing and quantity and we will advise lead time and any minimum order.

What is CNC Turning 5086 Aluminum and how is it done?

CNC Turning 5086 Aluminum refers to cNC turning rotates the workpiece against a single-point tool to produce cylindrical features, threads and grooves. Applied to 5086 Aluminum — lightweight with excellent machinability — VT machining produces each part to your CAD drawing, selecting parameters from your tolerance, finish and quantity requirements.